Summary
A low-migration ink claim is only one part of qualification: PET surface treatment, ink weight, UV dose, press speed, overprint layers and the final package determine real adhesion, cure and migration performance.
What happened
Flint Group reported on 13 November 2026 that its Flexocure LEAP UV flexographic ink system had won the Sustainable Innovation category at the 2026 British Coatings Federation Awards. The company describes the mercury-UV system as 100% solids and VOC-free, so ink is not lost through solvent evaporation during printing.
Flint Group also says the ink uses a new resin technology designed to significantly reduce the risk of photoinitiator migration for indirect food-contact packaging. The product is positioned for labels and flexible packaging and as part of an NC-free portfolio intended to support plastic recycling.
Why it matters
For printers using PET or BOPET, a 100%-solids UV system can change the production discussion around solvent handling, drying and applied ink yield. It can also reduce one source of process variability because curing depends on UV energy rather than solvent evaporation. Those benefits, however, do not prove that the ink will adhere to every PET surface or remain fully cured at every press condition.
Migration risk is a finished-article question. It depends on ink formulation, ink-film weight, lamp spectrum and dose, line speed, substrate barrier, print-side orientation, set-off, lamination and intended food or sensitive-goods use. A supplier’s “designed to reduce risk” statement should therefore trigger a validation plan—not be converted into an unconditional compliance or equivalence claim.
Buyer checklist
- Define the PET surface. Confirm corona or chemical treatment, treated side, dyne level, coating or primer, surface age and storage conditions.
- Map the cure window. Record lamp type, irradiance, energy dose, line speed, ink weight, colour density and the minimum cure margin across the web.
- Test adhesion after conversion. Check tape, rub, scratch and chemical resistance after printing, rewinding, slitting, lamination, forming and ageing.
- Assess migration on the final construction. Use the actual substrate, print orientation, adhesive, barrier layers, food simulants and intended conditions of use.
- Verify the recyclability statement. Ask what “NC-free” means for the supplied series and which recycling protocol, ink-removal or compatibility evidence supports the claim.
- Control production changes. Require notification for formulation, pigment, photoinitiator, resin, manufacturing-site or curing-guidance changes that could affect qualification.